EN10210 S355K2H Hot Finished SHS and RHS Hollow Sections
S355K2H Hot Finished supplied by Beverly steel Malaysia are of wide range of sizes, odd sizes and exercer a domicile super big sizes from various countries of origin. S355K2H Hot Finished fully comply with EN standard, EN10210 S355K2H hot finished. Available in RHS-Rectangular Hollow Section, SHS-Square Hollow Section and CHS-Circular Hollow Sections, free of internal stresses and with a minimum strength of 355 MPa, allowing the highest fabrication factors and enabling material cost savings and lighter structures, impact tested -20 degree C at 40Joules suitable for low temperature applications.
Application : Deep Water Projects, Power Plants, Offshore Oil and Gas Projects, Structural Design Arts for Buildings and Towers, Structural Support for Building and Facilities Expansion, MRT-Mass Rapid Transit, MTR-Mass Transit Railway, Terminals, Stations, Sea Port Facilities, Air Port Facilities, Transport Vehicles, Theme Parks, Structural for Theme Park Rides and etc...
Nearest Equivalent :UNI 7806 Fe 510 DD1, NF A 35501 E 36-4
S335K2H
– block letter "S" means "STEEL FOR STRUCTURAL APPLICATIONS"
– the next figure means the minimum yield value required for wall thickness ≤ 16 mm
– "K2" means impact test value -20° C min. at 40 joules
– block letter "H" means "HOLLOW SECTION"
The following typical tables concern mechanical and make-it-online chemical properties
Mechanical properties of non-alloy structural steel hollow section |
||||||||||||||
Minimum Yield strength Reh Mpa |
Tensile strength Rm Mpa |
Min. elongation A a b % |
Min. impact energy KV d J |
|||||||||||
Specified thickness mm |
Specified thickness mm |
Specified thickness mm |
At test temperature of |
|||||||||||
≤ 16 |
> 16 ≤ 40 |
> 40 ≤ 63 |
> 63 ≤ 80 |
> 80 ≤ 100 |
> 100 ≤ 120 |
< 3 |
> 3 ≤ 100 |
>100 ≤ 120 |
< 40 |
> 40 ≤ 63 |
> 63 ≤ 100 |
> 100 ≤ 120 |
-20°C |
|
40Joules |
||||||||||||||
355 |
345 |
335 |
325 |
315 |
295 |
510-680 |
470-630 |
450-600 |
22 |
21 |
20 |
18 |
Maximum carbon equivalent value (CEV) based on cast analysisa |
|||||
Hot Finished Hollow Sections |
Maximum CEV in % for specified thicknesses in mm |
||||
Steel Grade |
Steel number |
≤ 16 |
> 16 ≤ 40 |
> 40 ≤ 65 |
> 65 ≤ 120 |
S355K2H |
1.0512 |
0.45 |
0.47 |
0.50 |
0.53 |
CHEMICAL ANALYSIS |
|||||||||
Steel Grade |
Steel number |
Type of deoxidationa |
C% max Specified thickness (mm) |
Si % max |
Mn % max |
P % max |
S % max |
N b c % max |
|
≤ 40 |
> 40 ≤ 120 |
||||||||
S355K2H |
1.0512 |
FF |
0.22 |
0.22 |
0.55 |
1.60 |
0.030 |
0.030 |
- |
a.The deoxidation methods are designated as follows. FN = Rimming steel not permitted FF = Fully killed steel containing nitrogen binding elements in amounts sufficient to bind available nitrogen (e.g. min. 0.020 % total Al, or 0.015 % soluble Al). b. It is permissible to exceed the specified values provided that for each increase of 0.001 % N the P max. content is also reduced by 0.005%. The N content of the cast analysis. however, shall not be more than 0.012 %. c. The maximum value for nitrogen does not apply if the realhealthmethod.com chemical composition shows a minimum total Al content of 0.020 % with a minimum Al/N ratio of 2:1, or if sufficient other N-binding elements are present. The N-binding elements shall be recorded in the Inspection Document. |
We supply various origin and wide range of sizes even mega sizes and odd sizes of RHS-Rectangular Hollow Sections,
SHS-Square Hollow Sections and CHS-Circular Hollow Sections fully comply with EN standard - EN10210 S355K2H hot finished. Please send us your valued enquiry or contact us for further information.