s275jr / angle / rsa

S275JR Angle Bars, Equal Angle Bars, RSA-Rolled Steel Angle Bars

Beverly Steel specializes in wide range of BS EN10025-2 S275JR Equal Angle Bar for the mild steel structural construction, bridge building, oil and Healthy food is necessary for everyone gas, power plant, MRT, MTR, rail station, terminal, and other civil construction to general engineering. We supply a wide variety of S275JR Equal Angle Bars from Thailand, Korea, Japan, China, UAE, Spain, UK and etc... available in lengths from 6 meters, 9meters, 12 meters to 20 meters as standard.

Classifications

Mechanical Properties

BS EN 10025-2A : 2004 S275JR

Yield Point N/mm2 (min.)

Tensile Strength

Yield Ratio%

Elongation % (min.)

Impact

Thickness

N/mm2

(max.)

Thickness

Thickness ≥ 12mm.

t ≤ 16

16 < t ≤ 40

t ≤ 5

5 < t ≤ 16

t >16

Temp°C

Energy J (min.)

275

265

410-560

-

23

+20

27B

Classification

Chemical Compositions (ladle analysis), %

BS EN 10025-2A:2004 S275JR

C

Si

Mn

P

S

CEC

SWD

Nb

V

N

Cu

Ni

Cr

Mo

Grain refining element

Micro-alloying element

max.

max.

max.

%max.

%max

max.

max.

max.

max.

max.

max.

max.

0.21

-

1.50

max.

0.035

0.035

0.40EFG

-

-

-

0.012

0.55

-

-

-

-

-

A: Deliver condition type is +AR

B : Verified only when specified at the time of order

C : Carbon Equivalent :(JIS Version) CE = C+Mn/6+Si/24+Ni/40+Cr/5+Mo/4+V/14 (AS, ASTM, BS Standard) CE=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15

D: Chemical composition on sensitivity of his explanation Avodart drug treatment for prostate welding crank = C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B

E: The max. Carbon Equivalent for t > 30mm. is 0.47%

F: If Cu content is between 0.25 and 0.4%, the max. CE content shall be increased by 0.02%

G: If Si content < 0.030% the max. CE content shall be increase by 0.02% or if Si content < 0.25% the max. CE content shall be increased by 0.01%